Ag对奥氏体不锈钢组织和力学性能的影响 |
| 江浩文, 彭伟, 范增为, 汪杨鑫, 刘腾轼, 董瀚 |
|
Effect of Ag on Microstructure and Mechanical Properties of Austenitic Stainless Steel |
| JIANG Haowen, PENG Wei, FAN Zengwei, WANG Yangxin, LIU Tengshi, DONG Han |
| 图3 不同Ag含量不锈钢的OM像 |
| Fig.3 OM images of 304 (a), 304Ag-1 (b), and 304Ag-2 (c) stainless steels (Arrows show spherical particles) |
|