GCr15钢滚动轴承疲劳剥落失效过程中一种针状相的形成 |
| 程胜, 孙阳, 赵文辉, 栾义坤, 郑成武, 李殿中 |
|
Formation of a Needle-Like Structure when Surface Flaking Occurs During the Rolling Contact Fatigue of a GCr15 Bearing |
| CHENG Sheng, SUN Yang, ZHAO Wenhui, LUAN Yikun, ZHENG Chengwu, LI Dianzhong |
| 图7 单一针状相内部微观结构的TEM像 |
| Fig.7 TEM bright-field image (a) and HRTEM image (b) of one specific needle-like structure, locally high magnified HRTEM image of the square area indicated in Fig.7b (c) (Inset in Fig.7c shows the corresponding FFT diffractogram) |
|