低温轧制对高强高导Cu-1Cr-0.2Zr-0.25Nb合金性能及析出行为的影响
|
|
李龙健, 李仁庚, 张家郡, 曹兴豪, 康慧君, 王同敏
|
Effects of Cryorolling on Properties and Precipitation Behavior of a High-Strength and High-Conductivity Cu-1Cr-0.2Zr-0.25Nb Alloy
|
|
LI Longjian, LI Rengeng, ZHANG Jiajun, CAO Xinghao, KANG Huijun, WANG Tongmin
|
|
表3 屈服强度计算所用的参数
|
Table 3 Parameters used in yield strength calculation
|
|
| Parameter | Symbol | Unit | Value | Ref. |
|---|
| Shear modulus of Cu alloy | G | GPa | 44 | [35] | | Taylor factor | M | | 3.06 | [36] | | Burgers vector modulus | b | nm | 0.2556 | [35] | | Poisson's ratio | ν | | 0.33 | [37] | | Maximum volume fraction of precipitates | VCr-Max | % | 0.9 | This work | | Minimum value of conductivity | C0 | %IACS | 29.30 | This work | | Maximum value of conductivity | CMax | %IACS | 83.46 | This work | | Transformation fraction of precipitation for CRⅡ-FA300 sample | XCRII-FA300 | % | 93.26 | This work | | Volume fraction of the precipitates for CRⅡ-FA300 sample | fCRII-FA300 | % | 0.839 | This work | | Mean radius of the precipitates for CRⅡ-FA300 sample | rCRII-FA300 | nm | 6.1 | This work |
|
|
|