低温轧制对高强高导Cu-1Cr-0.2Zr-0.25Nb合金性能及析出行为的影响 |
| 李龙健, 李仁庚, 张家郡, 曹兴豪, 康慧君, 王同敏 |
|
Effects of Cryorolling on Properties and Precipitation Behavior of a High-Strength and High-Conductivity Cu-1Cr-0.2Zr-0.25Nb Alloy |
| LI Longjian, LI Rengeng, ZHANG Jiajun, CAO Xinghao, KANG Huijun, WANG Tongmin |
| 图8 RⅡ-FA300样品的TEM像 |
| Fig.8 TEM images of RⅡ-FA300 sample (a) deformation twin and detwinning (b) precipitates and subgrain |
|