低温轧制对高强高导Cu-1Cr-0.2Zr-0.25Nb合金性能及析出行为的影响 |
| 李龙健, 李仁庚, 张家郡, 曹兴豪, 康慧君, 王同敏 |
|
Effects of Cryorolling on Properties and Precipitation Behavior of a High-Strength and High-Conductivity Cu-1Cr-0.2Zr-0.25Nb Alloy |
| LI Longjian, LI Rengeng, ZHANG Jiajun, CAO Xinghao, KANG Huijun, WANG Tongmin |
| 图5 CRⅡ-FA300样品中析出相的TEM分析 |
| Fig.5 TEM analyses of precipitates in CRⅡ-FA300 sample (a) bright-field TEM image (Inset shows the SAED pattern of precipitates) (b) HRTEM image of precipitates (c, d) FFT images of precipitates of region A (c) and region B (d) in Fig.5b |
|