基于界面追踪-动网格技术模拟凝固收缩下Fe-C合金宏观偏析 |
| 董士虎, 张红伟, 吕文朋, 雷洪, 王强 |
|
Numerical Simulation on Macrosegregation in Fe-C Alloy Under Solidification Shrinkage Through Interface Tracking-Dynamic Mesh Technique |
| DONG Shihu, ZHANG Hongwei, LÜ Wenpeng, LEI Hong, WANG Qiang |
| 图6 铸锭中心线上溶质相对浓度分布 |
| Fig.6 Relative concentration distribution of C along ingot centerline (The experimental[ |
|