初始组织及冷轧压下量对工业低牌号电工钢相变织构及磁性能的影响 |
| 杨平, 马丹丹, 顾晨, 顾新福 |
|
Influence of Initial Microstructure and Cold Rolling Reduction on Transformation Texture and Magnetic Properties of Industrial Low-Grade Electrical Steel |
| YANG Ping, MA Dandan, GU Chen, GU Xinfu |
| 图1 样品轧制及退火工艺流程图 |
| Fig.1 Schematic of rolling and annealing process routes (Inset shows the schematic of microstructure of initial sample) |
|