δ-铁素体对钠冷快堆用316KD奥氏体不锈钢热变形行为和动态再结晶的影响 |
| 陈胜虎, 王琪玉, 姜海昌, 戎利建 |
|
Effect of δ-Ferrite on Hot Deformation and Recrystallization of 316KD Austenitic Stainless Steel for Sodium-Cooled Fast Reactor Application |
| CHEN Shenghu, WANG Qiyu, JIANG Haichang, RONG Lijian |
| 图9 铸态样品经应变为0.36压缩变形后的TEM像及元素分布图 |
| Fig.9 TEM bright field images (a, b) and corresponding elemental mapping (c) from the selected rectangular area indicated in Fig.9a of as-cast samples with the strain of 0.36 (Fig.9b shows the high magnification image at the lower left corner of the selected rectangular area in Fig.9a) |
|