δ-铁素体对钠冷快堆用316KD奥氏体不锈钢热变形行为和动态再结晶的影响 |
| 陈胜虎, 王琪玉, 姜海昌, 戎利建 |
|
Effect of δ-Ferrite on Hot Deformation and Recrystallization of 316KD Austenitic Stainless Steel for Sodium-Cooled Fast Reactor Application |
| CHEN Shenghu, WANG Qiyu, JIANG Haichang, RONG Lijian |
| 图4 lg{ln[1 / (1 - X(t))]}与lg{lnt}以及lnk与1 / T之间的拟合关系曲线 |
| Fig.4 lg{ln[1 / (1 - X(t))]} as a function of lg{lnt} (a) and lnk as a function of 1 / T (b) (T—homogenization temperature, X—area fraction of δ-ferrite, t—time, k—reaction rate constant) |
|