Al和Cr协同作用提高核用高强钢耐水蒸气氧化性能 |
|||||||||||||||||||||||
| 彭祥阳, 张乐, 李聪聪, 侯硕, 刘迪, 周建明, 路广遥, 蒋虽合 | |||||||||||||||||||||||
|
Synergetic Effects of Al and Cr on Enhancing Water Vapor Oxidation Resistance of Ultra-High Strength Steels for Nuclear Applications |
|||||||||||||||||||||||
| PENG Xiangyang, ZHANG Le, LI Congcong, HOU Shuo, LIU Di, ZHOU Jianming, LU Guangyao, JIANG Suihe | |||||||||||||||||||||||
| 表2 氧化前经时效处理的5Cr和9Cr试样在室温和600℃下的力学性能 |
|||||||||||||||||||||||
| Table 2 Mechanical properties of 5Cr and 9Cr samples aged at 500oC for 4 h before oxidation experiments at RT and 600oC |
|||||||||||||||||||||||
|
|||||||||||||||||||||||