Al和Cr协同作用提高核用高强钢耐水蒸气氧化性能 |
| 彭祥阳, 张乐, 李聪聪, 侯硕, 刘迪, 周建明, 路广遥, 蒋虽合 |
|
Synergetic Effects of Al and Cr on Enhancing Water Vapor Oxidation Resistance of Ultra-High Strength Steels for Nuclear Applications |
| PENG Xiangyang, ZHANG Le, LI Congcong, HOU Shuo, LIU Di, ZHOU Jianming, LU Guangyao, JIANG Suihe |
| 图1 氧化前经过时效处理的5Cr和9Cr试样的SEM像、XRD谱和拉伸应力-应变曲线 |
| Fig.1 SEM images of 5Cr (a) and 9Cr (b) samples aged at 500oC for 4 h before oxidation experiments, corresponding XRD spectra (c), and tensile stress-strain curves at room temperature (RT) and 600oC (d) |
|