航空用TC21钛合金变截面模锻件的显微组织和力学性能不均匀性分析
杨杰, 黄森森, 尹慧, 翟瑞志, 马英杰, 向伟, 罗恒军, 雷家峰, 杨锐

Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation
YANG Jie, HUANG Sensen, YIN Hui, ZHAI Ruizhi, MA Yingjie, XIANG Wei, LUO Hengjun, LEI Jiafeng, YANG Rui
表3 图1a中Ⅱ和Ⅴ处沿不同方向的拉伸和冲击性能
Table 3 Tensile and impact properties at positions Ⅱ and Ⅴ in Fig.1a along LD and ND
PositionDirectionRp0.2 / MPaRm / MPaA / %Z / %I / J
ⅡLD1063 ± 51198 ± 109.0 ± 1.514.0 ± 2.533.0 ± 2.0
ND1043 ± 31185 ± 58.0 ± 2.010.0 ± 3.530.9 ± 2.1
ⅤLD1014 ± 21137 ± 311.3 ± 1.716.0 ± 2.440.0 ± 2.0
ND1013 ± 31138 ± 46.5 ± 2.511.0 ± 3.036.0 ± 3.5