航空用TC21钛合金变截面模锻件的显微组织和力学性能不均匀性分析 |
| 杨杰, 黄森森, 尹慧, 翟瑞志, 马英杰, 向伟, 罗恒军, 雷家峰, 杨锐 |
|
Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation |
| YANG Jie, HUANG Sensen, YIN Hui, ZHAI Ruizhi, MA Yingjie, XIANG Wei, LUO Hengjun, LEI Jiafeng, YANG Rui |
| 图12 图1a中Ⅱ处沿不同方向的典型拉伸断口形貌 |
| Fig.12 Typical tensile fracture morphologies at position Ⅱ in Fig.1a along LD (a-c) and ND (d-f) (Insets show the side macro-morphologies of the corresponding tensile fracture) |
|