航空用TC21钛合金变截面模锻件的显微组织和力学性能不均匀性分析 |
| 杨杰, 黄森森, 尹慧, 翟瑞志, 马英杰, 向伟, 罗恒军, 雷家峰, 杨锐 |
|
Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation |
| YANG Jie, HUANG Sensen, YIN Hui, ZHAI Ruizhi, MA Yingjie, XIANG Wei, LUO Hengjun, LEI Jiafeng, YANG Rui |
| 图7 图1a中Ⅱ处高倍SEM像和α + β取向图及相应极图 |
| Fig.7 High magnified SEM image and corresponding α + β orientation maps and pole figures at position Ⅱ in Fig.1a (a) microstructure of the αp and βt (b) corresponding β orientation map (c) corresponding α orientation map (d) pole figures |
|