航空用TC21钛合金变截面模锻件的显微组织和力学性能不均匀性分析 |
| 杨杰, 黄森森, 尹慧, 翟瑞志, 马英杰, 向伟, 罗恒军, 雷家峰, 杨锐 |
|
Inhomogeneity Analyses of Microstructure and Mechanical Properties of TC21 Titanium Alloy Variable Cross-section Die Forgings for Aviation |
| YANG Jie, HUANG Sensen, YIN Hui, ZHAI Ruizhi, MA Yingjie, XIANG Wei, LUO Hengjun, LEI Jiafeng, YANG Rui |
| 图5 图1a中Ⅱ~Ⅵ处的β相的取向分布函数(ODF)图(φ2 = 45°) |
| Fig.5 Sections (φ2 = 45°) of orientation distribution function (ODF) maps of β phase at positions Ⅱ (a), Ⅲ (b), Ⅴ (c), and Ⅵ (d) in Fig.1a (φ1, φ2, Φ—Euler angles) |
|