脉冲电流辅助等离子弧焊Al-Mg合金晶粒细化机理 |
| 袁涛, 赵晓虎, 蒋晓青, 任学磊, 李博阳 |
|
Mechanism of Grain Refinement of Pulse Current Assisted Plasma Arc Welded Al-Mg Alloy |
| YUAN Tao, ZHAO Xiaohu, JIANG Xiaoqing, REN Xuelei, LI Boyang |
| 图2 传统脉冲电流等离子弧焊焊缝上表面偏光图 |
| Fig.2 Polarization micrographs of upper surface of conventional pulse current PAW (a) C0 (b) S1 (c) S2 (d) S3 (e) S4 (f) S5 |
|