多道次压缩变形对AZ80镁合金微观组织演化的影响 |
| 李振亮, 张欣磊, 田董扩 |
|
Effect of Multi-Pass Compression Deformation on Microstructure Evolution of AZ80 Magnesium Alloy |
| LI Zhenliang, ZHANG Xinlei, TIAN Dongkuo |
| 图2 恒温、阶梯降温2类变形工艺的微观组织演变 |
| Fig.2 Microstructure evolutions of constant-temperature deformation process at ε = 0.2 (a), ε = 0.4 (b), and ε = 0.6 (c); and step-cooling deformation process at ε = 0.6 (d) |
|