GH3535合金焊缝高温氦离子辐照效应 |
| 白菊菊, 李健健, 付崇龙, 陈双建, 李志军, 林俊 |
|
Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature |
| BAI Juju, LI Jianjian, FU Chonglong, CHEN Shuangjian, LI Zhijun, LIN Jun |
| 图10 辐照前后母材和焊缝的硬度随压入深度变化及 |
| Fig.10 Nanohardness vs indentation depth (a, b) and H 2-1/ h curves (c, d) of the base metal (a, c) and weld metal (b, d) before and after irradiation |
|