Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature |
| BAI Juju, LI Jianjian, FU Chonglong, CHEN Shuangjian, LI Zhijun, LIN Jun |
| 图8 弱束TEM明暗场下焊缝中峰值区域的位错环分布(850℃) |
| Fig.8 Weak-beam dark-field ( g /3 g ) TEM image (a) and bright-field TEM image (b) of the dislocation loops in the peak region of the weld metal at 850oC (The dislocation loops appear as white dots under the weak beam dark-field condition, and becomes black dots at the same position under the bright-field as shown in the red circles; the same in Fig.9) |
|