GH3535合金焊缝高温氦离子辐照效应 |
| 白菊菊, 李健健, 付崇龙, 陈双建, 李志军, 林俊 |
|
Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature |
| BAI Juju, LI Jianjian, FU Chonglong, CHEN Shuangjian, LI Zhijun, LIN Jun |
| 图4 母材中He泡随氦离子辐照深度的分布 |
| Fig.4 Distributions of helium bubble with the irradiation depth of the base metal at 850oC (a) cross-sectional TEM image at lower magnification (b1, b2) enlarged images of the 800-1400 nm region in under-focus (b1) and over-focus (b2) conditions, respectively |
|