GH3535合金焊缝高温氦离子辐照效应 |
| 白菊菊, 李健健, 付崇龙, 陈双建, 李志军, 林俊 |
|
Effect of He Ion Irradiation on the GH3535 Weld Metal at High Temperature |
| BAI Juju, LI Jianjian, FU Chonglong, CHEN Shuangjian, LI Zhijun, LIN Jun |
| 图2 焊缝和母材的EBSD晶粒图、SEM像以及TEM下位错线和碳化物分布 |
| Fig.2 EBSD maps (inverse pole figures) (a, d), SEM images (b, e), and bright-field TEM images (c1, c2, f1, f2) for the weld metal (a, b, c1, c2) and base metal (d, e, f1, f2), where Figs.2c1 and f1 show the dislocations in weld and base metal, respectively, Figs.2c2 and f2 show the carbides in weld and base metal, respectively |
|