轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能 |
| 蒋招汉, 邱文婷, 龚深, 李周 |
|
Preparation and Properties of Lightweight HfO2@CNT/Polymer/CuAlMn Composite with High Strength and High Damping |
| JIANG Zhaohan, QIU Wenting, GONG Shen, LI Zhou |
| 图4 5种材料的损耗因子和储能模量室温下随频率变化曲线和100 Hz下随温度变化曲线;多孔CuAlMn SMA、CNT/聚合物/CuAlMn和HfO2@CNT/聚合物/CuAlMn复合材料的损耗因子和储能模量在1、10和100 Hz下随温度的变化曲线;5种材料室温下的压缩应力-应变曲线 |
| Fig.4 Curves of five materials' loss factors and storage moduli with frequency at room temperature (a) and temperature at 100 Hz (b); temperature dependence curves of loss factors and storage moduli of porous CuAlMn SMA (c), CNT/polymer/CuAlMn (d), and HfO2@CNT/polymer/CuAlMn (e) at 1, 10, and 100 Hz; compressive stress-strain curves at room temperature of five materials (f) |
|