轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能 |
| 蒋招汉, 邱文婷, 龚深, 李周 |
|
Preparation and Properties of Lightweight HfO2@CNT/Polymer/CuAlMn Composite with High Strength and High Damping |
| JIANG Zhaohan, QIU Wenting, GONG Shen, LI Zhou |
| 图2 淬火态多孔CuAlMn SMA和聚合物/CuAlMn复合材料的SEM像,淬火态多孔CuAlMn SMA的室温XRD谱,远离孔隙、孔隙边缘以及典型孪晶马氏体的TEM像,及I区域的HRTEM像和选区电子衍射花样 |
| Fig.2 SEM images of quenched porous CuAlMn SMA (a, b) and polymer/CuAlMn composite (c); XRD spectrum of quenched porous CuAlMn SMA at room temperature (M—martensite with M18R structure) (d); TEM images of the areas away from pores (e) and around pores (f), and typical twin martensite (g) of quenched porous CuAlMn SMA; HRTEM image (h) and SAED pattern (i) of the area I in Fig.2g |
|