轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能 |
| 蒋招汉, 邱文婷, 龚深, 李周 |
|
Preparation and Properties of Lightweight HfO2@CNT/Polymer/CuAlMn Composite with High Strength and High Damping |
| JIANG Zhaohan, QIU Wenting, GONG Shen, LI Zhou |
| 图1 HfO2@CNT/聚合物/CuAlMn复合材料的制备流程示意图(CNT代表碳纳米管) |
| Fig.1 Schematic of preparation process of HfO2@CNT/polymer/CuAlMn composite (The abbreviations CNT and SMA represent carbon nanotube and shape memory alloy, respectively) |
|