超声冲击对增材制造组织改善及强化机理影响的研究进展 |
| 孙徕博, 黄陆军, 黄瑞生, 徐锴, 武鹏博, 龙伟民, 姜风春, 方乃文 |
|
Progress in the Effect of Ultrasonic Impact Treatment on Microstructure Improvement and Strengthening Mechanism in Additive Manufacturing |
| SUN Laibo, HUANG Lujun, HUANG Ruisheng, XU Kai, WU Pengbo, LONG Weimin, JIANG Fengchun, FANG Naiwen |
| 图2 超声冲击作用下SMA490BW钢组织演变及其示意图[ |
| Fig.2 SMA490BW steel microstructural evolutions and schematics influenced by UIT[ (a) microstructure without treatment (b) dislocation multiplication (c) formation of dislocation cells (d) formation of subgrains (e) microstructure refinement |
|