钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图11 拉伸断裂后纵截面界面区域的EBSD分析 (a) SEM image (b) phase distribution map (c) EBSD orientation map (d) EBSD KAM color map with respect to ρGND (e) {01 |
| Fig.11 EBSD results of the fractured Al84Ni7Gd6Co3/TC4 composite near the interface along tensile direction |
|