钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图10 Al84Ni7Gd6Co3/TC4复合材料断口形貌的SEM像 |
| Fig.10 Low (a) and locally high magnified fracture SEM images of areas Ⅰ (b), Ⅱ (c), and Ⅲ (d) of Al84Ni7Gd6Co3/TC4 composite |
|