钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图8 Al84Ni7Gd6Co3/TC4复合材料和纯Al84Ni7Gd6Co3纳米结构铝合金的拉伸性能,及本工作和目前报道[ |
| Fig.8 Tensile true stress-strain curves of the Al84Ni7Gd6Co3/TC4 composite and the pure Al84Ni7Gd6Co3 alloy (Insets in Fig.8a show the corresponding photographs of tensile samples) (a) and comparisons between the present materials and the other reported Ti/Al composites with the ultimate tensile strength as a function of density (Data for the other materials are taken from the literatures [24,39-61]. AMC—aluminum-based matrix composite) (b) |
|