钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图7 Al84Ni7Gd6Co3/TC4复合材料纵截面界面区域的EBSD分析结果 (a) SEM image (b) phase distribution map (c) EBSD orientation map (d) EBSD kernel average misorientation (KAM) color map with respect to the geometrically necessary dislocation (GND) density (ρGND) (e) {01 |
| Fig.7 EBSD results of the Al84Ni7Gd6Co3/TC4 composite near the interface along extrusion direction |
|