钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图6 Al84Ni7Gd6Co3/TC4复合材料的界面特征 (a, b) low (a) and high (b) magnified SEM images (Inset in Fig.6b shows the EDS results of point 1) (c) EDS line scanning result along line in Fig.6b |
| Fig.6 SEM analyses of the Al84Ni7Gd6Co3/TC4 composite near the interface |
|