钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图5 Al84Ni7Gd6Co3/TC4复合材料横截面和纵截面的微观组织 (a, b) OM images of the transversal section (a) and longitudinal section (b) (c) BSE-SEM image of the Al84Ni7Gd6Co3 alloy area of transversal section (d, e) SE-SEM images of the TC4 lattice showing the microstructures of the transversal section (d) and longitudinal section (e) |
| Fig.5 Microstructures of the Al84Ni7Gd6Co3/TC4 composite |
|