钛合金三维点阵结构增韧纳米铝合金的力学性能和变形行为 |
| 王勇, 张卫文, 杨超, 王智 |
|
Mechanical Properties and Deformation Behavior of a Nanostructured Aluminum Alloy Toughened by Titanium Alloy Base Three-Dimensional Lattice Structure |
| WANG Yong, ZHANG Weiwen, YANG Chao, WANG Zhi |
| 图2 热挤压制备Al84Ni7Gd6Co3/TC4复合材料的示意图 (a) cold press (b) hot extrusion (c) hot extruded sample (d) dimension of the tensile sample (unit: mm) |
| Fig.2 Schematic showing the used processing route for manufacturing Al84Ni7Gd6Co3/TC4 composite |
|