复合磁场对金属熔体流动及凝固组织的影响 |
| 朱锐, 王俊杰, 张云虎, 田志超, 苗信成, 翟启杰 |
|
Flow and Solidification Microstructure in Metal Melts Driven by a Combined Magnetic Field |
| ZHU Rui, WANG Junjie, ZHANG Yunhu, TIAN Zhichao, MIAO Xincheng, ZHAI Qijie |
| 图17 磁场方向、感应电流方向和感应电流环路面积示意图 (a) PMO (b) CMF |
| Fig.17 Schematics of magnetic field direction, induced electric current direction, and induced electric current loop area (SP and SC are the areas of the induced current loop under the application of PMO and CMF, respectively ) |
|