复合磁场对金属熔体流动及凝固组织的影响 |
| 朱锐, 王俊杰, 张云虎, 田志超, 苗信成, 翟启杰 |
|
Flow and Solidification Microstructure in Metal Melts Driven by a Combined Magnetic Field |
| ZHU Rui, WANG Junjie, ZHANG Yunhu, TIAN Zhichao, MIAO Xincheng, ZHAI Qijie |
| 图3 流场测量示意图 |
| Fig.3 Schematic of melt flow measurement setup (H0 and D0 are the height and diameter of the cylindrical container respectively; H2 is the melt height; h is the distance between the bottom of the container and the bottom of the coil; UDV—ultrasound Doppler velocimetry; P1 is the position of the probe at the bottom of the container) |
|