含氧纳米多晶 α-Ti拉伸力学性能与变形机制的分子动力学模拟 |
任军强, 邵珊, 王启, 卢学峰, 薛红涛, 汤富领 |
Molecular Dynamics Simulation of Tensile Mechanical Properties and Deformation Mechanism of Oxygen-Containing Nano-Polycrystalline α-Ti |
REN Junqiang, SHAO Shan, WANG Qi, LU Xuefeng, XUE Hongtao, TANG Fuling |
图13 不同温度下多晶Ti-0.3O拉伸过程bcc原子占比与应变关系 |
Fig.13 Relationship between proportion of bcc atoms and strain during tension of polycrystalline Ti-0.3O at different temperatures |
![]() |