微米级选区激光熔化316L不锈钢的拉伸力学性能 |
||||||||||||
| 张楠, 张海武, 王淼辉 | ||||||||||||
|
Tensile Mechanical Properties of Micro-Selective Laser Melted 316L Stainless Steel |
||||||||||||
| ZHANG Nan, ZHANG Haiwu, WANG Miaohui | ||||||||||||
| 表1 M-SLM成形316L不锈钢不同增材方向的拉伸性能 |
||||||||||||
| Table 1 Tensile properties of M-SLMed 316L stainless steel with different building directions |
||||||||||||
|
||||||||||||