微米级选区激光熔化316L不锈钢的拉伸力学性能 |
| 张楠, 张海武, 王淼辉 |
|
Tensile Mechanical Properties of Micro-Selective Laser Melted 316L Stainless Steel |
| ZHANG Nan, ZHANG Haiwu, WANG Miaohui |
| 图10 微矩形截面法判定 (a) Σ3 grain boundary (b) pole figure of {111} crystal form |
| Fig.10 Schematic of Σ3 grain boundary determination on the circle area in Fig.8b using micro rectangular section method ( N1 and N2 represent normal directions adjacent to grain boundaries of rectangle 1 and rectangle 2, respectively) |
|