微米级选区激光熔化316L不锈钢的拉伸力学性能 |
| 张楠, 张海武, 王淼辉 |
|
Tensile Mechanical Properties of Micro-Selective Laser Melted 316L Stainless Steel |
| ZHANG Nan, ZHANG Haiwu, WANG Miaohui |
| 图6 M-SLM和传统SLM成形316L不锈钢拉伸力学性能比较 |
| Fig.6 Comparisons of tensile properties of M-SLMed 316L stainless steel and fabricated by traditional SLM |
|