NiAl和Cu在40CrNi3MoV钢中的析出行为及其对力学性能的影响
梁恩溥, 徐乐, 王毛球, 时捷

Precipitation Behavior of NiAl and Cu in 40CrNi3MoV Steel and Its Effect on Mechanical Properties
LIANG Enpu, XU Le, WANG Maoqiu, SHI Jie
图4 500℃回火后P-Al钢和P-Al + Cu钢中析出相的HRTEM像和FFT衍射图
Fig.4 HRTEM images (a, c) and Fourier fast transform (FFT) diffraction patterns (b, d) of precipitates in P-Al experimental steel (a, b) and P-Al + Cu experimental steel (c, d) after tempering at 500oC (Insets are partial enlarged views of the precipitated phase)