NiAl和Cu在40CrNi3MoV钢中的析出行为及其对力学性能的影响 |
梁恩溥, 徐乐, 王毛球, 时捷 |
Precipitation Behavior of NiAl and Cu in 40CrNi3MoV Steel and Its Effect on Mechanical Properties |
LIANG Enpu, XU Le, WANG Maoqiu, SHI Jie |
图3 500℃回火后的P-Al + Cu钢的TEM像和EDS元素分布图 |
Fig.3 TEM image of the matrix with grain boundaries (a) and EDS element maps showing the distributions of Al element (green) (b), Cu element (blue) (c), and Ni, Al and Cu elements (Ni is red) (d) of P-Al + Cu steel tempered at 500oC |
![]() |