冷轧中锰钢的再结晶调控及其对力学性能的影响 |
| 胡宝佳, 郑沁园, 路轶, 贾春妮, 梁田, 郑成武, 李殿中 |
|
Recrystallization Controlling in a Cold-Rolled Medium Mn Steel and Its Effect on Mechanical Properties |
| HU Baojia, ZHENG Qinyuan, LU Yi, JIA Chunni, LIANG Tian, ZHENG Chengwu, LI Dianzhong |
| 图6 0.15C-5Mn冷轧MMS经不同温度预退火并ART处理及常规ART处理试样的工程应力-应变曲线 |
| Fig.6 Engineering stress-strain curves of the cold-rolled 0.15C-5Mn MMS treated by various thermal cycles |
|