冷轧中锰钢的再结晶调控及其对力学性能的影响 |
| 胡宝佳, 郑沁园, 路轶, 贾春妮, 梁田, 郑成武, 李殿中 |
|
Recrystallization Controlling in a Cold-Rolled Medium Mn Steel and Its Effect on Mechanical Properties |
| HU Baojia, ZHENG Qinyuan, LU Yi, JIA Chunni, LIANG Tian, ZHENG Chengwu, LI Dianzhong |
| 图3 0.15C-5Mn冷轧MMS在不同临界区温度预退火处理后微观组织的EBSD分析 |
| Fig.3 EBSD band contrast images (a-c) and kernel average misorientation (KAM) maps (d-f) of the cold-rolled 0.15C-5Mn MMS pre-annealed at 680oC (a, d), 700oC (b, e), and 720oC (c, f) (The red, green, and blue lines represent boundaries with misorientations of 2° < θ < 5°, 5° ≤ θ < 15°, and θ ≥ 15°, respectively) |
|