GH4151镍基高温合金 μ 相中的基面层错 |
|||||||||
| 龙江东, 段慧超, 赵鹏, 张瑞, 郑涛, 曲敬龙, 崔传勇, 杜奎 | |||||||||
|
Basal Stacking Faults of μ Phase in Ni-Based Superalloy GH4151 |
|||||||||
| LONG Jiangdong, DUAN Huichao, ZHAO Peng, ZHANG Rui, ZHENG Tao, QU Jinglong, CUI Chuanyong, DU Kui | |||||||||
| 表1 C14和C15结构的形成能 (meV·atom-1) |
|||||||||
| Table 1 Formation energies of C14 and C15 structures |
|||||||||
|
|||||||||