GH4151镍基高温合金 μ 相中的基面层错 |
| 龙江东, 段慧超, 赵鹏, 张瑞, 郑涛, 曲敬龙, 崔传勇, 杜奎 |
|
Basal Stacking Faults of μ Phase in Ni-Based Superalloy GH4151 |
| LONG Jiangdong, DUAN Huichao, ZHAO Peng, ZHANG Rui, ZHENG Tao, QU Jinglong, CUI Chuanyong, DU Kui |
| 图3 μ相的低倍高角度环形暗场扫描透射电子显微镜(HAADF-STEM)像及EDS元素分布图 |
| Fig.3 Low magnification high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) image (a) and EDS element maps of μ phase (b-f) |
|