一种第四代镍基单晶高温合金的同相位热机械疲劳行为及损伤机制 |
|||||||||||||||
| 谭子昊, 李永梅, 王新广, 赵浩川, 谭海兵, 王标, 李金国, 周亦胄, 孙晓峰 | |||||||||||||||
|
In-Phase Thermal-Mechanical Fatigue Behavior and Damage Mechanism of a Fourth-Generation Ni-Based Single-Crystal Superalloy |
|||||||||||||||
| TAN Zihao, LI Yongmei, WANG Xinguang, ZHAO Haochuan, TAN Haibing, WANG Biao, LI Jinguo, ZHOU Yizhou, SUN Xiaofeng | |||||||||||||||
| 表1 DD91合金在不同应变幅下IP-TMF断裂后的外表面最长裂纹尺寸及内部裂纹数量 |
|||||||||||||||
| Table 1 Maximum crack sizes on outer surface and numbers of internal crack of the DD91 alloy after IP-TMF fracture at different strain amplitudes |
|||||||||||||||
|
|||||||||||||||