基于稳定性的第三代先进高强钢设计 |
| 张宇, 吴盼, 贾东昇, 黄林科, 贾晓晴, 刘峰 |
|
TG-AHSS Materials Design Based on Thermodynamic and Generalized Stability |
| ZHANG Yu, WU Pan, JIA Dongsheng, HUANG Linke, JIA Xiaoqing, LIU Feng |
| 图5 基于热-动力学相关性和广义稳定性的热-动力学贯通性的定性展示[ |
| Fig.5 Qualitative demonstration of thermo-kinetic coherence based on thermo-kinetic correlation and generalized stability (GS)[ |
|