基于稳定性的第三代先进高强钢设计 |
| 张宇, 吴盼, 贾东昇, 黄林科, 贾晓晴, 刘峰 |
|
TG-AHSS Materials Design Based on Thermodynamic and Generalized Stability |
| ZHANG Yu, WU Pan, JIA Dongsheng, HUANG Linke, JIA Xiaoqing, LIU Feng |
| 图2 不同热处理工艺下第三代先进高强钢力学性能的比较[ |
| Fig.2 Comparison of mechanical properties of third-generation of advanced high strength steel (TG-AHSS) in different heat treatment processing[ |
|