基于稳定性的第三代先进高强钢设计
张宇, 吴盼, 贾东昇, 黄林科, 贾晓晴, 刘峰

TG-AHSS Materials Design Based on Thermodynamic and Generalized Stability
ZHANG Yu, WU Pan, JIA Dongsheng, HUANG Linke, JIA Xiaoqing, LIU Feng
图1 热-动力学相关性与广义稳定性的定性展示[36]
Fig.1 Qualitative demonstration of thermo-kinetic correlations and generalized stability (Δ) [36] (ΔG*, ΔG—thermodynamic driving force of reference and final states (in phase transition or deformation), respectively; Q*, Q —kinetic energy barrier of reference and final states (in phase transition or deformation), respectively)