含Zr镁合金晶粒细化机理与研究进展
刘勇, 曾刚, 刘洪, 王煜, 李建龙

Grain Refinement Mechanism and Research Progress of Magnesium Alloy Incorporating Zr
LIU Yong, ZENG Gang, LIU Hong, WANG Yu, LI Jianlong
表1 镁合金中常用溶质元素的生长限制因子(Q)[25,45,46,58]
Table 1 Growth restriction factors (Q) of common solute elements in magnesium alloys[25,45,46,58]
ElementQElementQ
Fe52.56[45]Nd3.557[25]
Zr38.29[45]Sm2.943[25]
Ca11.94[45]Pr2.909[25]
Si9.25[45]La2.895[25]
Ni6.13[45]Tb2.073[25]
Zn5.31[45]Eu2.490[25]
Cu5.28[45]Gd1.025[25]
Ge4.41[45]Ho0.860[25]
Al4.32[45]Dy0.828[25]
Sb0.53[45]Tm0.557[25]
Mn0.15[45]Er0.524[25]
Sr3.51[58]Lu0.123[46]
Ce2.74[58]Na6.878[46]
Sc3.96[58]Pd4.070[46]
Yb2.53[58]Co3.178[46]
Y1.70[58]Ag2.675[46]
Sn1.47[58]Cd2.644[46]
Pb1.03[58]Li2.034[46]