微纳米Ti2AlC增强TiAl复合材料高温强韧化机制 |
| 陈占兴, 王玉鹏, 荣光飞, 张新房, 马腾飞, 王晓红, 邢秋玮, 朱冬冬 |
|
High-Temperature Strengthening and Toughening Mechanisms of Micro-Nano Ti2AlC Reinforced TiAl Composites |
| CHEN Zhanxing, WANG Yupeng, RONG Guangfei, ZHANG Xinfang, MA Tengfei, WANG Xiaohong, XING Qiuwei, ZHU Dongdong |
| 图8 1300℃烧结的TiAl合金高温拉伸断口附近变形组织的SEM像 |
| Fig.8 Low (a, b) and locally high (a1, b1) magnified SEM images of TiAl alloy sintered at 1300oC after tensile tests at 800oC(a, a1) and 850oC (b, b1) |
|